Di(2-Ethylhexyl) Peroxydicarbonate 75% - Leading China Suppliers & Factory for Polymerization Initiators

EHP is a highly effective initiator, containing 75% active ingredient, specifically designed for the (co)polymerization of ethylene, vinyl chloride, and vinylidene chloride. As a leading product from our factory in China, we proudly serve as reliable suppliers for various industries seeking high-quality polymerization solutions. Choose EHP for optimal performance in your polymerization processes, backed by our commitment to excellence and innovation

    Half Life Data

    10 Hours 47℃
    1 Hour 64℃
    1 Minute 83℃
    PRODUCT3dbe
    EHP 75% Details
    Chemical Name Di(2-ethylhexyl) peroxydicarbonate
    Molecular Formula C18H34O6
    Molecular Weight 246.5
    CAS NO. 16111-62-9
    UN NO. 3115
    EINECS 240-282-4

    Specification

    Property Specification Value
    Appearance clear liquid
    Assay 74.0-76.0 %
    Active Oxygen Content 3.41-3.51 %

    Package & Storage

    Standard packaging size for EHP is 20 kg net. Smaller packaging size is available on request.
    • Store in a cool and ventilated space, with the warehouse temperature not exceeding -15℃.
    • Stay away from the fire and the heat source. It shall be stored separately from acid, reducing agent, flammable, combustible, reducing agent, etc.
    • The lighting and ventilation facilities in the storage room are explosion-proof, and the switch is located outdoors.
    • When handling, you should be careful to prevent the damage of packaging and containers, prohibit impact and oscillation, and pay attention to personal protection in packing and handling operations.
    • Please read the Safety Technical Manual (MSDS) carefully when storing, transporting and using the product.
    Thermal Stability Warning
    Organic peroxides are thermally unstable substances, which may undergo self-accelerating decomposition. The lowest temperature at which self-accelerating decomposition of a substance in the original packaging may occur is the Self Accelerating Decomposition Temperature (SADT). The SADT is determined on the basis of the Heat Accumulation Storage Test.
    SADT
    5°C (41°F)
    Emergency Temp (Tₑ)
    -5°C (23°F)
    Control Temp (Tc)
    -15°C (5°F)
    Method: The Heat Accumulation Storage Test is a recognized test method for the determination of the SADT of organic peroxides (see Recommendations on the Transport of Dangerous Goods, Manual of Tests and Criteria - United Nations, New York and Geneva).

    Applications

    EHP is an efficient initiator for the production of Low Density Polyethylene (LDPE). It is used both for tubular and autoclave processes. In most cases a combination with other peroxides is used to ensure a broad reactivity range. EHP is applied as an initiator for the suspension and mass polymerization of vinyl chloride in the temperature range between 40°C and 65°C.

    Frequently Asked Questions

    What is the chemical name and CAS number of EHP 75%?
    The chemical name of EHP 75% is Di(2-ethylhexyl) peroxydicarbonate, and its CAS number is 16111-62-9. Its molecular formula is C18H34O6.
    What are the half-life temperatures of EHP?
    The half-life temperatures for EHP are 47℃ for 10 hours, 64℃ for 1 hour, and 83℃ for 1 minute.
    How should EHP be stored safely?
    EHP must be stored in a cool, ventilated space with warehouse temperatures not exceeding -15℃. Keep it away from fire and heat sources, stored separately from acids, reducing agents, flammables, and combustibles. Ensure explosion-proof lighting and ventilation facilities are used.
    What are the SADT, emergency, and control temperatures for EHP?
    For EHP, the Self Accelerating Decomposition Temperature (SADT) is 5°C (41°F), the emergency temperature (Te) is -5°C (23°F), and the control temperature (Tc) is -15°C (5°F).
    What are the primary applications of EHP?
    EHP is primarily used as an efficient initiator for producing Low Density Polyethylene (LDPE) in both tubular and autoclave processes, as well as an initiator for the suspension and mass polymerization of vinyl chloride within a temperature range of 40°C to 65°C.

    Leave Your Message